dc.contributor.author | Napari, Mari | |
dc.contributor.author | Lahtinen, Manu | |
dc.contributor.author | Veselov, Alexey | |
dc.contributor.author | Julin, Jaakko | |
dc.contributor.author | Østreng, Erik | |
dc.contributor.author | Sajavaara, Timo | |
dc.date.accessioned | 2017-08-08T07:33:44Z | |
dc.date.available | 2019-07-25T21:36:01Z | |
dc.date.issued | 2017 | |
dc.identifier.citation | Napari, M., Lahtinen, M., Veselov, A., Julin, J., Østreng, E., & Sajavaara, T. (2017). Room-temperature plasma-enhanced atomic layer deposition of ZnO : Film growth dependence on the PEALD reactor configuration. <i>Surface and Coatings Technology</i>, <i>326</i>(Part A, October), 281-290. <a href="https://doi.org/10.1016/j.surfcoat.2017.07.056" target="_blank">https://doi.org/10.1016/j.surfcoat.2017.07.056</a> | |
dc.identifier.other | CONVID_27135356 | |
dc.identifier.other | TUTKAID_74534 | |
dc.identifier.uri | https://jyx.jyu.fi/handle/123456789/55011 | |
dc.description.abstract | Room-temperature plasma-enhanced atomic layer deposition (PEALD) of ZnO was studied by depositing the films using diethylzinc and O2 plasma from inductively-coupled plasma (ICP) and capacitively-coupled plasma (CCP) plasma source configurations. The CCP-PEALD was operated using both remote and direct plasma. It was observed that the films deposited by means of remote ICP and CCP were all highly oxygen rich, independently on plasma operation parameters, but impurity (H, C) contents could be reduced by increasing plasma pulse time and applied power. With the direct CCP-PEALD the film composition was closer to stoichiometric, and film crystallinity was enhanced. The ZnO film growth was observed to be similar on silicon, polycarbonate and poly(methyl methacrylate) substrates, but changes in polymer surface morphology indicate plasma-induced damage during the deposition due to exposure to ion bombardment when direct plasma was applied. | |
dc.language.iso | eng | |
dc.publisher | Elsevier Sequoia | |
dc.relation.ispartofseries | Surface and Coatings Technology | |
dc.subject.other | plasma-enhanced atomic layer deposition | |
dc.subject.other | inductively-coupled plasma | |
dc.subject.other | capacitively-coupled plasma | |
dc.title | Room-temperature plasma-enhanced atomic layer deposition of ZnO : Film growth dependence on the PEALD reactor configuration | |
dc.type | article | |
dc.identifier.urn | URN:NBN:fi:jyu-201708043412 | |
dc.contributor.laitos | Fysiikan laitos | fi |
dc.contributor.laitos | Kemian laitos | fi |
dc.contributor.laitos | Department of Physics | en |
dc.contributor.laitos | Department of Chemistry | en |
dc.contributor.oppiaine | Fysiikka | fi |
dc.contributor.oppiaine | Epäorgaaninen ja analyyttinen kemia | fi |
dc.contributor.oppiaine | Kiihdytinlaboratorio | fi |
dc.contributor.oppiaine | Physics | en |
dc.contributor.oppiaine | Inorganic and Analytical Chemistry | en |
dc.contributor.oppiaine | Accelerator Laboratory | en |
dc.type.uri | http://purl.org/eprint/type/JournalArticle | |
dc.date.updated | 2017-08-04T06:15:15Z | |
dc.type.coar | http://purl.org/coar/resource_type/c_2df8fbb1 | |
dc.description.reviewstatus | peerReviewed | |
dc.format.pagerange | 281-290 | |
dc.relation.issn | 0257-8972 | |
dc.relation.numberinseries | Part A, October | |
dc.relation.volume | 326 | |
dc.type.version | acceptedVersion | |
dc.rights.copyright | © 2017 Elsevier B.V. This is a final draft version of an article whose final and definitive form has been published by Elsevier. Published in this repository with the kind permission of the publisher. | |
dc.rights.accesslevel | openAccess | fi |
dc.subject.yso | sinkkioksidi | |
jyx.subject.uri | http://www.yso.fi/onto/yso/p27694 | |
dc.relation.doi | 10.1016/j.surfcoat.2017.07.056 | |
dc.type.okm | A1 | |