Näytä suppeat kuvailutiedot

dc.contributor.authorYlivaara, Oili M.E.
dc.contributor.authorLangner, Andreas
dc.contributor.authorLiu, Xuwen
dc.contributor.authorSchneider, Dieter
dc.contributor.authorJulin, Jaakko
dc.contributor.authorArstila, Kai
dc.contributor.authorSintonen, Sakari
dc.contributor.authorAli, Saima
dc.contributor.authorLipsanen, Harri
dc.contributor.authorSajavaara, Timo
dc.contributor.authorHannula, Simo-Pekka
dc.contributor.authorPuurunen, Riikka L.
dc.date.accessioned2021-06-14T10:07:55Z
dc.date.available2021-06-14T10:07:55Z
dc.date.issued2021
dc.identifier.citationYlivaara, O. M., Langner, A., Liu, X., Schneider, D., Julin, J., Arstila, K., Sintonen, S., Ali, S., Lipsanen, H., Sajavaara, T., Hannula, S.-P., & Puurunen, R. L. (2021). Mechanical and optical properties of as-grown and thermally annealed titanium dioxide from titanium tetrachloride and water by atomic layer deposition. <i>Thin Solid Films</i>, <i>732</i>, Article 138758. <a href="https://doi.org/10.1016/j.tsf.2021.138758" target="_blank">https://doi.org/10.1016/j.tsf.2021.138758</a>
dc.identifier.otherCONVID_89788531
dc.identifier.urihttps://jyx.jyu.fi/handle/123456789/76491
dc.description.abstractThe use of thin-films made by atomic layer deposition (ALD) is rapidly growing in the field of optical sensing. ALD TiO2 has been widely characterized for its physical and optical properties, but systematic information about the influence of thermal history to optical and mechanical properties of the film is lacking. Optical applications require planar surface and tunability of the refractive index and residual stress. In addition, mechanical properties such as elastic modulus and film hardness influence the performance of the layer, especially, when optics is integrated with microelectromechanical systems. In this work, optical properties, density, elemental analysis, residual stress, elastic modulus and hardness of as-grown ALD TiO2 thin films on silicon were studied at temperature range from 80 to 350 °C and influence of post-ALD annealing to films were studied on films annealed up to 900 °C. ALD TiO2 films were under tensile stress in the scale of hundreds of MPa. The stress depended both on the ALD temperature and film thickness in a complex way, and onset of crystallization increased the residual stress. Films grown at 110 and 300 °C were able to withstand post-ALD annealing at 420 °C without major change in residual stress, the refractive index or the extinction coefficient. Elastic modulus and hardness increased upon crystallization with increasing ALD temperature. The results presented here help to improve the design of the optical devices by choosing films with desired optical properties and help to design the post-ALD thermal budget so that films maintain their desired features.en
dc.format.mimetypeapplication/pdf
dc.language.isoeng
dc.publisherElsevier
dc.relation.ispartofseriesThin Solid Films
dc.rightsCC BY 4.0
dc.titleMechanical and optical properties of as-grown and thermally annealed titanium dioxide from titanium tetrachloride and water by atomic layer deposition
dc.typeresearch article
dc.identifier.urnURN:NBN:fi:jyu-202106143694
dc.contributor.laitosFysiikan laitosfi
dc.contributor.laitosDepartment of Physicsen
dc.contributor.oppiaineYdin- ja kiihdytinfysiikan huippuyksikköfi
dc.contributor.oppiaineFysiikkafi
dc.contributor.oppiaineCentre of Excellence in Nuclear and Accelerator Based Physicsen
dc.contributor.oppiainePhysicsen
dc.type.urihttp://purl.org/eprint/type/JournalArticle
dc.type.coarhttp://purl.org/coar/resource_type/c_2df8fbb1
dc.description.reviewstatuspeerReviewed
dc.relation.issn0040-6090
dc.relation.volume732
dc.type.versionpublishedVersion
dc.rights.copyright© 2021 the Authors
dc.rights.accesslevelopenAccessfi
dc.type.publicationarticle
dc.subject.ysofysikaaliset ominaisuudet
dc.subject.ysoatomikerroskasvatus
dc.subject.ysotitaanidioksidi
dc.subject.ysoohutkalvot
dc.subject.ysooptiset ominaisuudet
dc.format.contentfulltext
jyx.subject.urihttp://www.yso.fi/onto/yso/p1174
jyx.subject.urihttp://www.yso.fi/onto/yso/p27468
jyx.subject.urihttp://www.yso.fi/onto/yso/p24148
jyx.subject.urihttp://www.yso.fi/onto/yso/p16644
jyx.subject.urihttp://www.yso.fi/onto/yso/p25870
dc.rights.urlhttps://creativecommons.org/licenses/by/4.0/
dc.relation.doi10.1016/j.tsf.2021.138758
jyx.fundinginformationThis work was carried out within the MECHALD project funded by Tekes and is linked to the Finnish Centers of Excellence in Atomic Layer Deposition (ref. 251220) and Nuclear and Accelerator Based Physics (refs. 213503 and 251353) of the Academy of Finland.